Toho Tenax Besfight® MC Type II (12,000 Filament) Nickel Coated Carbon Fiber

Category Carbon , Carbon Fiber , Other Engineering Material , Composite Fibers
Manufacturer Toho Tenax Co., Ltd.
Trade Name Besfight®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Toho Tenax Besfight® MC Type II (12,000 Filament) Nickel Coated Carbon Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Besfight MC Polyacrylonitrile (PAN) based fiber combines the mechanical properties and flexibility of carbon fiber with the electrical conductivity of nickel. It does not delaminate even at the mechanical breaking point due to the good bond between the carbon fiber and nickel. Used in thermoplastic compounds for EMI shielding. Information provided by Toho Carbon Fibers, a wholly owned subsidiary of Toho Tenax Co., Ltd.
Physical Properties Metric English Comments
Density 3.40 g/cc
0.123 lb/in³
Thickness 0.500 microns
0.0197 mil
Ni Coating Thickness
Fiber Count 20800 dtex
18700 denier
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 3090 MPa
448000 psi
Elongation at Break 1.5 %
1.5 %
Tensile Modulus 216 GPa
31300 ksi
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000350 ohm-cm
0.0000350 ohm-cm