Polymer Property : Electrical Resistivity = 0.0000293 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000293 ohm-cm
0.0000293 ohm-cm
Lucas-Milhaupt Premabraze 130 Gold Based Brazing Alloy
Applications:Premabraze 130 can be used on any of the common nickel- and iron base heat-resistant alloys, such as in jet engines, etc. Because of its low penetration of the base metal, it is well s..
Electrical Resistivity 0.0000293 ohm-cm
0.0000293 ohm-cm
Lucas-Milhaupt Premabraze 131 Gold Based Brazing Alloy
Applications:Premabraze 131 can be used on any of the common nickel- and iron base heat-resistant alloys, such as in jet engines, etc. Because of its low penetration of the base metal, it is well s..