Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lucas-Milhaupt Premabraze 130 Gold Based Brazing Alloy

Category Metal , Nonferrous Metal , Precious Metal , Gold Alloy , Solder/Braze Alloy
Manufacturer Lucas-Milhaupt
Trade Name Premabraze
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucas-Milhaupt Premabraze 130 Gold Based Brazing Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications:Premabraze 130 can be used on any of the common nickel- and iron base heat-resistant alloys, such as in jet engines, etc. Because of its low penetration of the base metal, it is well suited for brazing thin section, such as thin-wall tubing or electronic vacuum tubes. It has also been used extensively for nuclear power applications, except in high flux regions and in contact with such liquid metals as sodium and potassium. Characteristics:Premabraze 130 wets a wide range of high temperature iron and nickel based alloys such as the stainless steels, A286, Inconel and Inconel X very well. It does not alloy excessively with these materials nor produce the severe intergranular penetration normally associated with the nickel based brazing alloys contained boron. A minimum brazing temperature of 1800°F (980°C) is suggested for furnace brazing in hydrogen or dissociated ammonia having a -4°F dew point or drier on 300 and 400 series stainless steels which do not contain additions of Ti or Al. Stainless steels of the 17-7 PH variety require dew points of -70°F or drier for furnace brazing. Brazing is done in inert atmospheres or in vacuum. For torch brazing, protection with Handy Hi-Temp Flux is recommended. Where base metals containing elements which produce refractory oxides are encountered, Handy Hi-Temp Flux Boron Modified will promote better wetting. Joint clearances of 0.0015" - 0.003" are normally suggested.Gold and nickel are completely soluble in all proportions at temperatures above 1490°F (810°C) and this specific composition (82% Au- 18% Ni) represents the minimum in this system so that the solidus (melting point) and the liquidus (flow point) are identical. Normally, Premabraze 130 would not be used for joining copper based and silver based alloys. In addition to have a flow point very close to the melting point of silver, and above that of the silver-copper eutectic, it would alloy quite readily with copper based alloys.Specifications:Premabraze 130 conforms to the following specifications: SAE-AMS 4787, AWS A5-8 BAu-4, ASME Boiler & Pressure Vessel Code Sec II-C SFA-5.8 BAu-4 Information provided by Lucas-Milhaupt, Inc.
Physical Properties Metric English Comments
Specific Gravity 15.82 g/cc
15.82 g/cc
Mechanical Properties Metric English Comments
Tensile Strength at Break 427 MPa

@Temperature 23.0 °C
62000 psi

@Temperature 73.4 °F
Tensile Strength, Ultimate 138 MPa

@Temperature 871 °C
20000 psi

@Temperature 1600 °F
Type 304 Stainless Steel butt joint
276 MPa

@Temperature 649 °C
40000 psi

@Temperature 1200 °F
Type 304 Stainless Steel butt joint
345 MPa

@Temperature 427 °C
50000 psi

@Temperature 800 °F
Type 304 Stainless Steel butt joint
Thermal Properties Metric English Comments
Melting Point 950.0 °C
1742 °F
Solidus 950.0 °C
1742 °F
Melting Point
Liquidus 950.0 °C
1742 °F
Flow Point
Component Elements Properties Metric English Comments
Gold, Au 81.5 - 82.5 %
81.5 - 82.5 %
Nickel, Ni 17.35 - 18.5 %
17.35 - 18.5 %
Other, total <= 0.15 %
<= 0.15 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000293 ohm-cm
0.0000293 ohm-cm
Processing Properties Metric English Comments
Processing Temperature 951.7 - 1010 °C
1745 - 1850 °F
Brazing Range
Descriptive Properties Value Comments
Color Nickel Gray
Copyright © lookpolymers.com All Rights Reserved