Electrical Properties Metric English Comments
Electrical Resistivity <= 0.0000287 ohm-cm
<= 0.0000287 ohm-cm
6% IACS conductivity (minimum)
Materion Beryllium Nickel Strip - Alloy 360 Hard, 1.5 hr at 950°F
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 1.5 hrs @ 510ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation..
Electrical Resistivity 0.0000287 - 0.0000573 ohm-cm
0.0000287 - 0.0000573 ohm-cm
3-6% IACS Conductivity
Materion Beryllium Nickel M220C
Information supplied by Brush Wellman Engineered Materials.Brush M220C is characterized by high levels of strength, hardness, and thermal conductivity combined with excellent resistance to wear, cor..
Electrical Resistivity <= 0.0000287 ohm-cm
<= 0.0000287 ohm-cm
6% IACS conductivity (minimum)
Materion Beryllium Nickel Strip - Alloy 360 1/2 Hard, 1.5 hr at 950°F
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 1.5 hrs @ 510ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation..
Electrical Resistivity <= 0.0000287 ohm-cm
<= 0.0000287 ohm-cm
6% IACS conductivity (minimum)
Materion Beryllium Nickel Strip - Alloy 360 1/4 Hard, 2.5 hr at 950°F
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 2.5 hrs @ 510ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation..
Electrical Resistivity <= 0.0000287 ohm-cm
<= 0.0000287 ohm-cm
6% IACS conductivity (minimum)
Materion Beryllium Nickel Strip - Alloy 360 Annealed, 2.5 hr at 950°F
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 2.5 hrs @ 510ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation..
Electrical Resistivity 0.0000287 ohm-cm
0.0000287 ohm-cm
6 % IACS
CMW® ELKONIUM 301 platinum based alloy
Platinum has complete freedom from atmospheric corrosion and is preferred for devices that have low closed forces and where surety of making a circuit may be a problem. It has a high melting point (..
Electrical Resistivity 0.0000287 ohm-cm
0.0000287 ohm-cm
6 % IACS
CMW® ELKONIUM 405 palladium based alloy
Palladium belongs to the platinum group of metals and like platinum is highly resistant to atmospheric corrosion; however, it begins to tarnish at temperatures above 400(C. It has a high melting poi..