Material Notes:
Palladium belongs to the platinum group of metals and like platinum is highly resistant to atmospheric corrosion; however, it begins to tarnish at temperatures above 400(C. It has a high melting point (1552(C) and, like platinum, resists arc formation. Its low electrical conductivity (16% IACS) limits its application to low current circuits. It costs much less than platinum, and is used as a lower cost alternative. Economics normally dictate that it be supplied as a composite contact with a thin contact metal facing silver brazed to a nickel-plated steel rivet, screw, or projection weld button backing.ELKONIUM® 405 is a palladium base alloy sold by CMW containing sufficient ruthenium to increase the hardness. Its corrosion resistance is similar to that of palladium and its resistance to transfer is greater than that of pure palladium. It is used in thermostats and other sensitive low voltage devices, and is a lower cost alternative to platinum alloys for these applications.Information provided by CMW Inc.
Physical Properties Metric English Comments
Density 12.0 g/cc
0.434 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell 15T 85
85
annealed
92
92
cold worked
Tensile Strength, Ultimate 483 MPa
70000 psi
annealed
689 MPa
100000 psi
cold worked
Elongation at Break 2.0 %
2.0 %
cold worked
13 %
13 %
annealed
Component Elements Properties Metric English Comments
Palladium, Pd 89 %
89 %
Ruthenium, Ru 11 %
11 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000287 ohm-cm
0.0000287 ohm-cm
6 % IACS