Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000248 - 0.0000260 ohm-cm | 0.0000248 - 0.0000260 ohm-cm | |
ATI Wah Chang Vanadium Vanadium is widely dispersed in the earths crust occurring in many types of deposits. Most vanadium is currently obtained as a by-product or co product from titanomagnetites, petroleum, uranium ores.. |