Material Notes:
Vanadium is widely dispersed in the earths crust occurring in many types of deposits. Most vanadium is currently obtained as a by-product or co product from titanomagnetites, petroleum, uranium ores, and phosphate rock. Table 1 shows the abundance of vanadium in the earths crust relative to some familiar elements.Applications: For many years, the major application for vanadium has been as a micro-alloying element for steel products. Added in amounts between 0.01% to 0.1%, vanadium lowers the ductile to brittle transition temperature of steel and increases toughness. Vanadium is currently being used in the production of high-strength low-alloy (HSLA) steels for applications in the automobile industry and the Alaskan pipeline where high strength to weight ratios are important.Information provided by ATI Wah Chang
Physical Properties Metric English Comments
Density 6.12 g/cc
0.221 lb/in³
Molecular Weight 50.942 g/mol
50.942 g/mol
Mechanical Properties Metric English Comments
Hardness, Brinell 60
60
Electron beam ingot
Tensile Strength, Ultimate 200 - 241 MPa
29000 - 35000 psi
Annealed Sheet
Tensile Strength, Yield 124 - 172 MPa

@Strain 0.200 %
18000 - 25000 psi

@Strain 0.200 %
Annealed Sheet
Elongation at Break 35 - 60 %
35 - 60 %
Annealed Sheet, in 2 inches
Modulus of Elasticity 137.9 GPa
20000 ksi
Poissons Ratio 0.36
0.36
Shear Modulus 50.7 GPa
7350 ksi
Calculated
Thermal Properties Metric English Comments
CTE, linear 8.30 µm/m-°C

@Temperature 23.0 - 100 °C
4.61 µin/in-°F

@Temperature 73.4 - 212 °F
Thermal Conductivity 30.914 W/m-K

@Temperature 100 °C
214.53 BTU-in/hr-ft²-°F

@Temperature 212 °F
Melting Point 1900 °C
3450 °F
Boiling Point 3400 °C
6150 °F
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000248 - 0.0000260 ohm-cm
0.0000248 - 0.0000260 ohm-cm
Magnetic Susceptibility 1.40e+6
1.40e+6
Paramagnetic
Critical Superconducting Temperature 4.46 K
4.46 K
H.R.E.
Chemical Properties Metric English Comments
Atomic Number 23
23
Processing Properties Metric English Comments
Recrystallization Temperature 800 - 1010 °C
1470 - 1850 °F