Electrical Properties Metric English Comments
Electrical Resistivity 0.0000148 ohm-cm
0.0000148 ohm-cm
Goodfellow Tin 60/Lead 39/Antimony 1 Alloy
A general purpose, low melting point soft solder which can also be used as a protective coating and for metal film capacitors.Information provided by Goodfellow.
Electrical Resistivity 0.0000148 ohm-cm
0.0000148 ohm-cm
Magnesium Elektron Elektron® 43 Magnesium Wrought Alloy
High strength wrought Mg alloy available as rolled plate, forging feedstock, and extrusions. It is a wrought evolution of the casting alloy Elektron WE43. Elektron 43 uses zirconium grain refining..