Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000147 ohm-cm | 0.0000147 ohm-cm | |
Indium Corp. Indalloy 1 Indium-Tin Solder Alloy Fair wettability on glass, quartz, and many ceramics. Good low temperature malleability. Compensates for some CTE mismatch. Low vapor pressureInformation Provided by Indium Corporation |
|||
Electrical Resistivity | 0.0000147 ohm-cm | 0.0000147 ohm-cm | |
Williams Advanced Alloys WS118 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |