Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000985 ohm-cm | 0.00000985 ohm-cm | (18% IACS) |
CMW® ELKONITE® TC53 Heat Treatable Tungsten Carbide Copper material For electroforging and electrical upsetting dies.Information provided by CMW Inc. |