Material Notes:
For electroforging and electrical upsetting dies.Information provided by CMW Inc.
Physical Properties Metric English Comments
Density 12.6 g/cc
0.455 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 47
47
Flexural Modulus 1.52 GPa
220 ksi
Thermal Properties Metric English Comments
Thermal Conductivity 120 W/m-K
833 BTU-in/hr-ft²-°F
Melting Point >= 980 °C
>= 1800 °F
Solidus 980 °C
1800 °F
Component Elements Properties Metric English Comments
Copper, Cu 28.22 %
28.22 %
Nickel, Ni 0.82 %
0.82 %
Silicon, Si 0.24 %
0.24 %
WC 70.12 %
70.12 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000985 ohm-cm
0.00000985 ohm-cm
(18% IACS)