Electrical Resistivity 0.00000750 - 0.00000810 ohm-cm
0.00000750 - 0.00000810 ohm-cm
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6
Heat Treatment Condition T6 (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo..
Electrical Resistivity 0.00000750 - 0.00000810 ohm-cm
0.00000750 - 0.00000810 ohm-cm
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6x
Heat Treatment Condition T6x (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials all..
Electrical Resistivity 0.00000750 - 0.00000960 ohm-cm
0.00000750 - 0.00000960 ohm-cm
18-23% IACS Conductivity
Materion Beryllium Copper Alloy 245C Castings (UNS C82600)
Pouring Temperature: 970-1065°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchTabula..
Electrical Resistivity 0.00000750 - 0.00000960 ohm-cm
0.00000750 - 0.00000960 ohm-cm
18-23% IACS Conductivity
Materion Beryllium Copper Alloy 245CT Castings (UNS C82600)
Pouring Temperature: 970-1065°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchTabula..
Electrical Resistivity 0.00000750 ohm-cm
0.00000750 ohm-cm
Indium Corp. Indalloy® 290 In-Ag Solder Alloy
Indium with silver added to improve strength. Has the wettability and low-temperature malleability of indium. Particularly useful for cryogenic applications.Information provided by the manufacturer,..
Electrical Resistivity 0.00000750 ohm-cm
0.00000750 ohm-cm
Special Metals Nickel 270
A high-purity grade of nickel made by powder metallurgy. It has a low base hardness and high ductility. Its extreme purity is useful for components of hydrogen thyratrons. It is also used for ele..
Electrical Resistivity 0.00000750 ohm-cm
0.00000750 ohm-cm
Forgings (23 % IACS)
CMW® 73 Copper Alloy