Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000663 ohm-cm | 0.00000663 ohm-cm | |
Chicago Extruded Metals BioBrass® UNS C46400 Copper-Zinc-Tin Alloy Copper-Zinc-Tin Alloy (Naval Brass)Finished product available as bar, wire, rod, forged, or shapes.Chicago Extruded Metal temper codes: H01, H02, H04, M30Information provided by Chicago Extruded Met.. |
|||
Electrical Resistivity | 0.00000663 ohm-cm | 0.00000663 ohm-cm | |
Chicago Extruded Metals UNS C33500 Copper-Zinc-Lead Alloy Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available in bars.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals |
|||
Electrical Resistivity | 0.00000663 ohm-cm | 0.00000663 ohm-cm | |
Chicago Extruded Metals UNS C34000 Copper-Zinc-Lead Alloy Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available as bar or rod.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals |
|||
Electrical Resistivity | 0.00000663 ohm-cm | 0.00000663 ohm-cm | |
Chicago Extruded Metals UNS C34500 Copper-Zinc-Lead Alloy Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available in rods.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals |
|||
Electrical Resistivity | 0.00000663 ohm-cm | 0.00000663 ohm-cm | |
Chicago Extruded Metals UNS C35000 Copper-Zinc-Lead Alloy Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available as bar or rod.Chicago Extruded Metal temper codes: H01, H02, H04Information provided by Chicago Extruded Metals |
|||
Electrical Resistivity | 0.00000663 ohm-cm | 0.00000663 ohm-cm | |
Chicago Extruded Metals UNS C35300 Copper-Zinc-Lead Alloy Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available as bar or rod.Chicago Extruded Metal temper codes: H01, H02, H04Information provided by Chicago Extruded Metals |
|||
Electrical Resistivity | 0.00000663 ohm-cm | 0.00000663 ohm-cm | |
Chicago Extruded Metals UNS C36000 Copper-Zinc-Lead Alloy Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available as bar, wire, rod or shapes.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals |
|||
Electrical Resistivity | 0.00000663 ohm-cm | 0.00000663 ohm-cm | |
Chicago Extruded Metals UNS C48200 Copper-Zinc-Tin Alloy Copper-Zinc-Tin Alloy (Naval Brass)Finished product available as bar, rod, forged, or shapes.Chicago Extruded Metal temper codes: H01, H02, H04, M30Information provided by Chicago Extruded Metals |
|||
Electrical Resistivity | 0.00000663 ohm-cm | 0.00000663 ohm-cm | |
Chicago Extruded Metals UNS C48500 Copper-Zinc-Tin Alloy Copper-Zinc-Tin Alloy (Naval Brass)Finished product available as bar, rod, forged, or shapes.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals |
|||
Electrical Resistivity | 0.00000663 ohm-cm | 0.00000663 ohm-cm | |
Chicago Extruded Metals UNS C36010 Copper-Zinc-Lead Alloy Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available as bar, wire, rod or shapes.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals |