Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000526 - 0.00000625 ohm-cm | 0.00000526 - 0.00000625 ohm-cm | |
ALIMEX 5083 O/H111Aluminum Alloy Rolled Rolled aluminium material according to DIN EN standard. Information provided by ALIMEX GmbHAnnealed and slightly strain-hardened |
|||
Electrical Resistivity | 0.00000526 - 0.00000625 ohm-cm | 0.00000526 - 0.00000625 ohm-cm | |
ALIMEX PLANAL 5083 O/H111 Aluminum Alloy Aluminium rolled plates which have been machined on both sides. Has a precise surface finish and high tensile strength. The temper values and the material conditions are not changed by surface-machi.. |