Polymer Property : Electrical Resistivity = 0.00000526 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000526 - 0.00000625 ohm-cm
0.00000526 - 0.00000625 ohm-cm
ALIMEX 5083 O/H111Aluminum Alloy Rolled
Rolled aluminium material according to DIN EN standard. Information provided by ALIMEX GmbHAnnealed and slightly strain-hardened
Electrical Resistivity 0.00000526 - 0.00000625 ohm-cm
0.00000526 - 0.00000625 ohm-cm
ALIMEX PLANAL 5083 O/H111 Aluminum Alloy
Aluminium rolled plates which have been machined on both sides. Has a precise surface finish and high tensile strength. The temper values and the material conditions are not changed by surface-machi..