Polymer Property : Electrical Resistivity = 0.00000610 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000570 - 0.00000610 ohm-cm
0.00000570 - 0.00000610 ohm-cm
PEAK Werkstoff DISPAL S693 Aluminum Alloy, AlCu5Ti, Condition T6
High stiffness and elongation at rupture. Property data for Condition T6 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH
Electrical Resistivity 0.00000570 - 0.00000610 ohm-cm
0.00000570 - 0.00000610 ohm-cm
PEAK Werkstoff DISPAL S693 Aluminum Alloy, AlCu5Ti, Condition T4
High stiffness and elongation at rupture. Property data for Condition T4 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH