Polymer Property : Electrical Resistivity = 0.00000440 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000440 ohm-cm
0.00000440 ohm-cm
Alcoa Toolrite 2011®-T3 Aluminum
Weldability = D; Stress Corrosion Cracking Resistance = D; General Corrosion Resistance = D (A = best; E = worst). General 2011 characteristics and uses: Good machinability, especially free-cutting ..
Electrical Resistivity 0.00000440 ohm-cm
0.00000440 ohm-cm
Alcoa Toolrite 2011®-T4 Aluminum
Weldability = D; Stress Corrosion Cracking Resistance = D; General Corrosion Resistance = D (A = best; E = worst). General 2011 characteristics and uses: Good machinability, especially free-cutting ..
Electrical Resistivity 0.00000440 ohm-cm
0.00000440 ohm-cm
precipitation hardened (4 hr)
CLAL-MSX SICLANIC S® TF Quenched Copper Alloy, precipitation treated
SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver..
Electrical Resistivity 0.00000440 ohm-cm
0.00000440 ohm-cm
precipitation hardened (3 hr)
CLAL-MSX SICLANIC S® TH3 Quenched Copper Alloy, 1/2 Hard, precipitation treated
SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver..
Electrical Resistivity 0.00000440 ohm-cm
0.00000440 ohm-cm
precipitation hardened (3 hr)
CLAL-MSX SICLANIC S® TH4 Quenched Copper Alloy, 4/4 Hard, precipitation treated
SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver..
Electrical Resistivity 0.00000440 ohm-cm
0.00000440 ohm-cm
Alpase M-1™ Aluminum Mold Plate
M-1™ features and benefits include: Dimensional stability, fully weldable, anodizable, consistent hardness - regardless of size, can be nickel plated, good machinability, no heat treatment required..