Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000351 - 0.00000420 ohm-cm | 0.00000351 - 0.00000420 ohm-cm | Calculated from 41-49 %IACS |
Cadi 30WC Tungsten Copper Available in a variety of rounds, rectangles, and shapes.Information provided by Cadi Company. |