Material Notes:
Available in a variety of rounds, rectangles, and shapes.Information provided by Cadi Company.
Physical Properties Metric English Comments
Density 15.6 g/cc
0.564 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 99 - 104
99 - 104
Component Elements Properties Metric English Comments
Copper, Cu 20 %
20 %
Tungsten, W 80 %
80 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000351 - 0.00000420 ohm-cm
0.00000351 - 0.00000420 ohm-cm
Calculated from 41-49 %IACS
Descriptive Properties Value Comments
RMWA Class 12