Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000174 ohm-cm | 0.00000174 ohm-cm | (99% IACS) |
CMW® D158F Silver Graphite Contact Material For electrical contacts; reduced sticking, low frictionInformation provided by CMW Inc. |