Electrical Properties Metric English Comments
Insulation Resistivity 200 Megaohm/1000 m

@Temperature 70.0 °C
656 Megaohm/1000 ft

@Temperature 158 °F
IEC 60502
Solvay Specialty Polymers Cogegum® AFR/920 Polyolefin, Unspecified  (discontinued **)
Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without ..
Insulation Resistivity 200 Megaohm/1000 m

@Temperature 70.0 °C
656 Megaohm/1000 ft

@Temperature 158 °F
IEC 60502
Solvay Specialty Polymers Cogegum® AFR/920-UV Polyolefin, Unspecified  (Unverified Data**)
Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without ..
Insulation Resistivity 200 Megaohm/1000 m

@Temperature 90.0 °C
656 Megaohm/1000 ft

@Temperature 194 °F
IEC 60502
Solvay Specialty Polymers Cogegum® GFR/350 Polyolefin, Unspecified  (Unverified Data**)
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi..
Insulation Resistivity 200 Megaohm/1000 m

@Temperature 90.0 °C
656 Megaohm/1000 ft

@Temperature 194 °F
IEC 60502
Solvay Specialty Polymers Cogegum® GFR/360 Polyolefin, Unspecified  (Unverified Data**)
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi..
Insulation Resistivity 200 Megaohm/1000 m

@Temperature 90.0 °C
656 Megaohm/1000 ft

@Temperature 194 °F
IEC 60502
Solvay Specialty Polymers Cogegum® GFR/365 Polyolefin, Unspecified  (Unverified Data**)
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi..