Electrical Properties | Metric | English | Comments |
---|---|---|---|
Insulation Resistivity | 200 Megaohm/1000 m @Temperature 70.0 °C |
656 Megaohm/1000 ft @Temperature 158 °F |
IEC 60502 |
Solvay Specialty Polymers Cogegum® AFR/920 Polyolefin, Unspecified
(discontinued **) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Insulation Resistivity | 200 Megaohm/1000 m @Temperature 70.0 °C |
656 Megaohm/1000 ft @Temperature 158 °F |
IEC 60502 |
Solvay Specialty Polymers Cogegum® AFR/920-UV Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Insulation Resistivity | 200 Megaohm/1000 m @Temperature 90.0 °C |
656 Megaohm/1000 ft @Temperature 194 °F |
IEC 60502 |
Solvay Specialty Polymers Cogegum® GFR/350 Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |
|||
Insulation Resistivity | 200 Megaohm/1000 m @Temperature 90.0 °C |
656 Megaohm/1000 ft @Temperature 194 °F |
IEC 60502 |
Solvay Specialty Polymers Cogegum® GFR/360 Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |
|||
Insulation Resistivity | 200 Megaohm/1000 m @Temperature 90.0 °C |
656 Megaohm/1000 ft @Temperature 194 °F |
IEC 60502 |
Solvay Specialty Polymers Cogegum® GFR/365 Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |