Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 354 - 420 °C | 669 - 788 °F | Average value: 376 °C Grade Count:10 |
Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Carbon Fiber Filled". Each property range of values reported is minimum and .. |
|||
Melt Temperature | 390 - 420 °C | 734 - 788 °F | |
Solvay Specialty Polymers Hyflon® MFA® F1540 Perfluoropolymer Hyflon® MFA is a unique family of perfluoro polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame re.. |