Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 390 - 410 °C | 734 - 770 °F | |
Solvay Specialty Polymers EpiSpire® EP-340 Sulfone, High Temperature (HTS)
(Unverified Data**) EpiSpire® EP-340 is a high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 265°C (509°F) and a heat deflection temperature of 255°C (491°F), E.. |
|||
Melt Temperature | 390 - 410 °C | 734 - 770 °F | Stock Temperature |
Solvay Specialty Polymers Supradel® HTS-2630 High Temperature Sulfone Resin
(discontinued **) SUPRADEL HTS-2630 is a 30% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer.In addition to exceptional thermal performance, this resin has the other performance .. |
|||
Melt Temperature | 390 - 410 °C | 734 - 770 °F | Stock Temperature |
Solvay Specialty Polymers Supradel® HTS-2401 High Temperature Sulfone Resin
(discontinued **) Supradel HTS-2401 is a high-temperature high-performance amorphous sulfone polymer designed for use in reinforced high temperature thermoplastic formulations. With its glass transition temperature o.. |
|||
Melt Temperature | 390 - 410 °C | 734 - 770 °F | Stock Temperature |
Solvay Specialty Polymers Supradel® HTS-2420 High Temperature Sulfone Resin
(discontinued **) SUPRADEL HTS-2420 is a 20% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 245°C and a heat deflection temperature of 2.. |
|||
Melt Temperature | 390 - 410 °C | 734 - 770 °F | Stock Temperature |
Solvay Specialty Polymers Supradel® HTS-2430 High Temperature Sulfone Resin
(discontinued **) SUPRADEL HTS-2420 is a 20% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 245°C and a heat deflection temperature of .. |
|||
Melt Temperature | 390 - 410 °C | 734 - 770 °F | Stock Temperature |
Solvay Specialty Polymers Supradel® HTS-2600 High Temperature Sulfone Resin
(discontinued **) SUPRADEL HTS-2600 is a high-temperature, high-performance, amorphous, sulfone polymer. In addition to exceptional thermal performance, this resin has the other performance features and attributes t.. |
|||
Melt Temperature | 390 - 410 °C | 734 - 770 °F | Stock Temperature |
Solvay Specialty Polymers Supradel® HTS-2601 High Temperature Sulfone Resin
(discontinued **) Supradel HTS-2601 is a high-temperature high-performance amorphous sulfone polymer designed as a base resin for reinforced thermoplastic products. This exceptional thermal performance is available i.. |
|||
Melt Temperature | 390 - 400 °C | 734 - 752 °F | |
LATI Larpeek 10 GCE/600 PEEK, Glass/Mineral Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers / Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa .. |
|||
Melt Temperature | 390 - 410 °C | 734 - 770 °F | |
Solvay Specialty Polymers EpiSpire® EP-340 Sulfone, High Temperature (HTS) EpiSpire® EP-340 is a high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 265°C (509°F) and a heat deflection temperature of 255°C (491.. |
|||
Melt Temperature | 390 - 420 °C | 734 - 788 °F | |
Solvay Specialty Polymers Hyflon® MFA® F1540 Perfluoropolymer Hyflon® MFA is a unique family of perfluoro polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame re.. |
|||
Melt Temperature | 390 - 410 °C | 734 - 770 °F | Stock Temperature |
Solvay Specialty Polymers Supradel® HTS-2620 High Temperature Sulfone Resin
(discontinued **) SUPRADEL HTS-2620 is a 20% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer.In addition to exceptional thermal performance, this resin has the other performance .. |
|||
Melt Temperature | 390 - 410 °C | 734 - 770 °F | Stock Temperature |
Solvay Specialty Polymers Supradel® HTS-2400 High Temperature Sulfone Resin
(discontinued **) SUPRADEL HTS-2400 is a high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 245°C and heat deflection temperature of 235°C, this resin extends the.. |