Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 377 - 388 °C | 711 - 730 °F | |
PolyOne Edgetek® PK-10GF/000 Polyetheretherketone (PEEK) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |