Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 377 - 388 °C | 711 - 730 °F | |
PolyOne Edgetek® PK-10GF/000 Polyetheretherketone (PEEK) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Melt Temperature | 377 - 382 °C | 710 - 720 °F | Average value: 379 °C Grade Count:3 |
Overview of materials for PEKK, Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Reinforced". Each property range of values reported is minimum and maximum values of appropriate M.. |