Melt Temperature 327 - 371 °C
620 - 700 °F
Molding
PolyOne Edgetek® PI-1000 Polyetherimide (PEI)  (discontinued **)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..