Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 252 °C | 486 °F | |
Chem Polymer Chemlon 253 H Nylon 6, Impact Modified A medium viscosity impact modified, heat stabilized nylon 6 exhibiting improved toughness over general purpose nylon 6.Data provided by the manufacturer, Chem Polymer. |
|||
Melt Temperature | 252 °C | 486 °F | |
Chem Polymer Chemlon 267 Nylon 6, Impact Modified An extrusion grade copolymer nylon 6, providing good melt strength, impact, elongation, and flexibility. This grade provides excellent properties in most convoluted tubing or wire coating applicati.. |
|||
Melt Temperature | 252 °C | 486 °F | |
Chem Polymer Chemlon 282 Nylon 6, Flame Retarded A non-halogenated, unfilled nylon 6 used in electrical applications where improved flame retardancy is required. The compound has excellent moldability, good snap-fit properties and is available in.. |
|||
Melt Temperature | 252 °C | 486 °F | |
Chem Polymer Chemlon 280 Nylon 6, High Impact A highly impact modified nylon 6 exhibiting excellent toughness and flexibility.Data provided by the manufacturer, Chem Polymer. |