Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chem Polymer Chemlon 282 Nylon 6, Flame Retarded

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced, Flame Retardant
Manufacturer Chem Polymer
Trade Name Chemlon
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chem Polymer Chemlon 282 Nylon 6, Flame Retarded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A non-halogenated, unfilled nylon 6 used in electrical applications where improved flame retardancy is required. The compound has excellent moldability, good snap-fit properties and is available in a range of colors.Data provided by the manufacturer, Chem Polymer.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 69.0 MPa
10000 psi
ASTM D638
Elongation at Break 15 %
15 %
ASTM D638
Flexural Yield Strength 83.0 MPa
12000 psi
ASTM D790
Flexural Modulus 3.20 GPa
464 ksi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 215 °C
419 °F
ASTM D789
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Comparative Tracking Index >= 600 V
>= 600 V
CTI, V
Processing Properties Metric English Comments
Melt Temperature 252 °C
486 °F