Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 216 - 228 °C | 420 - 442 °F | ASTM D789 |
Niche Polymer PA6GF33BK Nylon 6, 33% Glass Fiber Filled Information provided by Niche Polymer |
|||
Melt Temperature | 216 - 228 °C | 420 - 442 °F | ASTM D789 |
Niche Polymer PA6GF33N Nylon 6, 33% Glass Fiber Filled Information provided by Niche Polymer |