Processing Properties Metric English Comments
Melt Temperature 388 - 399 °C
730 - 750 °F
PolyOne Edgetek® PK-30GF/000 Polyetheretherketone (PEEK)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Melt Temperature 388 - 399 °C
730 - 750 °F
Molding
PolyOne Edgetek® PK-20CF/000 Polyetheretherketone (PEEK), Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
Melt Temperature 388 °C
730 °F
Molding
PolyOne Edgetek® PK-30CF/000 Polyetheretherketone (PEEK), Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
Melt Temperature 388 - 399 °C
730 - 750 °F
Molding
PolyOne Edgetek® PK-30GF/000 HT Polyaryletherketone, Glass Filled  (discontinued **)
Description/Features:30% Glass FilledPolyOne First ChoiceInformation provided by PolyOne Corporation.
Melt Temperature 388 - 399 °C
730 - 750 °F
Molding
PolyOne Edgetek® PK-40CF/000 Polyetheretherketone (PEEK), Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
Melt Temperature 388 - 421 °C
730 - 790 °F
Molding
PolyOne Edgetek® PI-40CF/000 Polyetherimide (PEI), Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.