Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 388 - 421 °C | 730 - 790 °F | Molding |
PolyOne Edgetek® PI-40CF/000 Polyetherimide (PEI), Carbon Fiber Reinforced