Polymer Property : Melt Temperature = 381 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 182 - 194 °C
360 - 381 °F
Huntsman PE1061 Film Extrusion Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: Exceptional strength, good machinability and heat seal characteristics.Applications: Film extrusion: high clarity packaging, frozen food, produce bags, shrink..
Melt Temperature 182 - 194 °C
360 - 381 °F
Huntsman PE1076 Film Extrusion Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: Yields film with high clarity and excellent stiffness.Applications: Film extrusion: overwrap packaging.FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (..
Melt Temperature 182 - 194 °C
360 - 381 °F
Huntsman PE1078 Film Extrusion Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: Yields film with high clarity and excellent stiffness.Applications: Film extrusion: overwrap packaging.FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (..