Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 182 - 194 °C | 360 - 381 °F | |
Huntsman PE1061 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Exceptional strength, good machinability and heat seal characteristics.Applications: Film extrusion: high clarity packaging, frozen food, produce bags, shrink.. |
|||
Melt Temperature | 182 - 194 °C | 360 - 381 °F | |
Huntsman PE1076 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Yields film with high clarity and excellent stiffness.Applications: Film extrusion: overwrap packaging.FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (.. |
|||
Melt Temperature | 182 - 194 °C | 360 - 381 °F | |
Huntsman PE1078 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Yields film with high clarity and excellent stiffness.Applications: Film extrusion: overwrap packaging.FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (.. |