Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 291 - 321 °C | 556 - 610 °F | Extrusion |
Albis Plastics Tedur® L V 9900-1 PPS, Unreinforced
(discontinued **) Excellent Surface Finish, High Chemical Resistance. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Pipes, ProfilesProcessing: Extrusion (Melt Temperature: 555-610°F).. |