Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Albis Plastics Tedur® L V 9900-1 PPS, Unreinforced  (discontinued **)

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS), Unreinforced, Extruded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Albis Plastics Tedur® L V 9900-1 PPS, Unreinforced  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent Surface Finish, High Chemical Resistance. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Pipes, ProfilesProcessing: Extrusion (Melt Temperature: 555-610°F)Tedur® is manufactured by Albis Plastics Corporation under license of the registered trademark owner (Bayer.) Data supplied by Albis Plastics Corporation.
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
DIN 53 47
Mechanical Properties Metric English Comments
Tensile Strength at Break 70.0 MPa
10200 psi
DIN 53 455
Elongation at Break 3.5 %
3.5 %
DIN 53 455
Modulus of Elasticity 3.20 GPa
464 ksi
DIN 53 457
Flexural Yield Strength 135 MPa
19600 psi
DIN 53 452
Flexural Modulus 3.20 GPa
464 ksi
DIN 53 457
Izod Impact, Notched 2.51 J/cm
4.70 ft-lb/in
Approximation; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 260 °C
500 °F
ASTM D648
Flammability, UL94 V-0
V-0
Albis North America Internal Test
Processing Properties Metric English Comments
Melt Temperature 291 - 321 °C
556 - 610 °F
Extrusion