Polymer Property : Melt Temperature = 2270 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 1090 - 1240 °C
2000 - 2270 °F
Wieland Porta SMK 82 PFM Alloy
Gold-palladium ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, removable partials, ceramic veneering, acrylic veneeringDental
Melt Temperature 1100 - 1240 °C
2010 - 2270 °F
Wieland Portalloy 54 PFM Alloy
Gold-palladium ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, removable partialsDental