Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 1090 - 1240 °C | 2000 - 2270 °F | |
Wieland Porta SMK 82 PFM Alloy Gold-palladium ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, removable partials, ceramic veneering, acrylic veneeringDental |
|||
Melt Temperature | 1100 - 1240 °C | 2010 - 2270 °F | |
Wieland Portalloy 54 PFM Alloy Gold-palladium ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, removable partialsDental |