Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 166 - 176 °C | 331 - 349 °F | |
PolyOne Geon™ Vinyl Wire & Cable Y594B Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |