Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 1210 - 1290 °C | 2210 - 2350 °F | |
Wieland Simidur Superior PFM Alloy Palladium-base ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, removable partialsDental |