Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 43200 - 86400 min @Temperature 40.0 °C |
43200 - 86400 min @Temperature 104 °F |
|
Abatron AboCast/AboCure 8109-12 1-part, contains latent hardener activated by higher temperature. 4-6 month shelf life at 20-25°C (68-77°F). Other versions available with longer shelf lives and cure cycles.Processing: Potlife:.. |