Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 1440 - 2880 min @Temperature 40.0 °C |
1440 - 2880 min @Temperature 104 °F |
|
Abatron AboCast/AboCure 8109-10 2-part, clear, slow casting/impregnating dielectric compound. Low dielectric constant, good flexibility and thermocycling properties. Abocast 8502-4 is a red (and other colors), filled version.Pro.. |