Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Pot Life 1440 - 2880 min

@Temperature 40.0 °C
1440 - 2880 min

@Temperature 104 °F
Abatron AboCast/AboCure 8109-10
2-part, clear, slow casting/impregnating dielectric compound. Low dielectric constant, good flexibility and thermocycling properties. Abocast 8502-4 is a red (and other colors), filled version.Pro..