Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | >= 172800 min @Temperature 20.0 °C |
>= 172800 min @Temperature 68.0 °F |
>4 months |
Abatron AboCast/AboCure 8109-12 1-part, contains latent hardener activated by higher temperature. 4-6 month shelf life at 20-25°C (68-77°F). Other versions available with longer shelf lives and cure cycles.Processing: Potlife:.. |