Polymer Property : Pot Life = 150 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Pot Life 150 min

@Temperature 20.0 °C
150 min

@Temperature 68.0 °F
Abatron AboCast/AboCure 8109-3
Low viscosity, RT cure. Easy processing.Processing: 100/10 pbw; Potlife: 2.5 h/20°C (68°F), 30 min/40°C (105°F), 15 min/60°C (140°F); mix at RT; cures in: 24 h/20°C (68°F), 2-3 h/60°C (140..
Pot Life 150 min

@Temperature 20.0 °C
150 min

@Temperature 68.0 °F
Abatron AboCast/AboCure 8109-4
Safety hardener (minimum toxicity) version of 8109-3.Processing: 100/10 pbw; Potlife: 2.5 h/20°C (68°F), 30 min/40°C (105°F), 15 min/60°C (140°F); mix at RT; cures in: 24 h/20°C (68°F), 2-3 ..
Pot Life 150 - 180 min

@Temperature 20.0 - 25.0 °C
150 - 180 min

@Temperature 68.0 - 77.0 °F
Abatron AboCast/AboCure 7606-1 Epoxy
AboCast 7606-1 is a transparent, light amber resin with a weight of 9.5 lbs/gallon and a viscosity of 2100 cps approx. @ 25°C. AboCure 7606-1 is a transparent, light amber converter with a weight o..