Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Pot Life = 120 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Pot Life 120 min

@Temperature 20.0 - 25.0 °C
120 min

@Temperature 68.0 - 77.0 °F
Abatron AboCast/AboCure 8006-11 Epoxy
AboCast/AboCure 8006-11 is a clear dielectric casting, adhesive, and encapsulating compound. It is a 2-component, radiation-resistant, low-viscosity plasticized epoxy system. It is virtually unaffec..