Polymer Property : Gel Time = 2.00 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Gel Time 2.00 - 8.00 min
2.00 - 8.00 min
Park Electrochemical Nelcote® E-718 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-718 is a modified epoxy resin system. E-718 is designed to provide excellent mechanical properties at low cure pressures.Key Features and Benefits:Good low pressure consolidationExcellen..
Gel Time 2.00 - 8.00 min
2.00 - 8.00 min
Park Electrochemical Nelcote® E-718 Epoxy Prepreg, G30-700 Uni-Tape Reinforced
Nelcote® E-718 is a modified epoxy resin system. E-718 is designed to provide excellent mechanical properties at low cure pressures.Key Features and Benefits:Good low pressure consolidationExcellen..
Gel Time 2.00 - 8.00 min
2.00 - 8.00 min
Park Electrochemical Nelcote® E-718 Epoxy Prepreg, T-700 24K Uni-Tape Reinforced
Nelcote® E-718 is a modified epoxy resin system. E-718 is designed to provide excellent mechanical properties at low cure pressures.Key Features and Benefits:Good low pressure consolidationExcellen..
Gel Time 2.00 - 6.00 min
2.00 - 6.00 min
Park Electrochemical Nelcote® E-763 Epoxy Prepreg, 3K 2x2 Twill Carbon Reinforced
Nelcote® E-763 is a modified epoxy system with a nominal 250°F cure temperature. E-763 provides a transparent resin surface on the finished part which gives finished part surfaces a cosmetic attra..
Gel Time 2.00 - 6.00 min
2.00 - 6.00 min
Park Electrochemical Nelcote® E-763 Epoxy Prepreg, 3K PW Carbon Reinforced
Nelcote® E-763 is a modified epoxy system with a nominal 250°F cure temperature. E-763 provides a transparent resin surface on the finished part which gives finished part surfaces a cosmetic attra..
Gel Time 2.00 - 6.00 min
2.00 - 6.00 min
Park Electrochemical Nelcote® E-763 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-763 is a modified epoxy system with a nominal 250°F cure temperature. E-763 provides a transparent resin surface on the finished part which gives finished part surfaces a cosmetic attra..
Gel Time 2.00 - 6.00 min

@Temperature 135 °C
2.00 - 6.00 min

@Temperature 275 °F
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, 120 E-Glass Reinforced
Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request...
Gel Time 2.00 - 6.00 min

@Temperature 135 °C
2.00 - 6.00 min

@Temperature 275 °F
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, 34-700 12K 2x2 Twill Reinforced
Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request...
Gel Time 2.00 - 6.00 min

@Temperature 135 °C
2.00 - 6.00 min

@Temperature 275 °F
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, T700 12K 2x2 Twill Reinforced
Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request...
Gel Time 2.00 - 6.00 min

@Temperature 135 °C
2.00 - 6.00 min

@Temperature 275 °F
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, T700 12K BW Reinforced
Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request...
Gel Time 2.00 min
2.00 min
Northstar Polymers MSB-D60A High Performance Polyurethane Cast Elastomer System
This is an Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires some lord bearing, high tensile strength, cut/tear res..
Gel Time 2.00 - 9.00 min

@Temperature 177 °C
2.00 - 9.00 min

@Temperature 351 °F
Hexcel® HexPly® F263 Epoxy Resin
HexPly® F263 is a structural, heat resistant epoxy resin formulated for excellent translation of high modulus carbon fiber properties in typically aerospace applications. HexPly® F263 is a high te..
Gel Time <= 2.00 min

@Temperature 135 °C
<= 2.00 min

@Temperature 275 °F
6
Hexcel® HexPly® F515 Epoxy Resin
HexPly® F515 is an advanced, industrial grade, modified epoxy formulation designed for either vacuum bag or autoclave curing to offer very high laminate strengths, coupled with increased fracture t..
Gel Time 2.00 min
2.00 min
ACC EP AJS EPI Engineered Polymers Aliphatic Joint Sealant
EP AJS Aliphatic Joint Sealant, “Powered by Reactamine® Technology, is a two component 100% solid, aliphatic (silicone optional) polyurea based joint sealant. EP AJS is a self-leveling joint seala..
Gel Time 2.00 min
2.00 min
Slow
ACC EP RAP EPI Engineered Polymers Aliphatic Silicone Polyurea
EP RAP Aliphatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Aliphatic Polyurea (silicone optional) that has excellent UV stability (colorfast) with supe..
Gel Time 2.00 min
2.00 min
Medium
ACC EP RASP EPI Engineered Polymers Aliphatic Silicone Polymer
EP RASP Aliphatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea that has excellent UV stability (colorfast) with superior performance in industria..
Gel Time 2.00 min

@Temperature 93.0 °C
2.00 min

@Temperature 199 °F
10 g
Abatron AboCast 8110-5/AboCure 8110-1 Flexible Epoxy
This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic..
Gel Time 2.00 min
2.00 min
2:1
ACC EP JS EPI Engineered Polymers Joint Sealant
EP JS Joint Sealant JS, “Powered by Reactamine® Technology” is a two component 100% solid (silicone optional) polyurea based joint sealant. EP JS is a self-leveling joint sealant designed to prot..