Processing Properties Metric English Comments
Annealing Temperature 1080 - 1160 °C
1980 - 2120 °F
Solution Annealing
Outokumpu 904L High Performance Austenitic Stainless Steel
Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar..