Processing Properties | Metric | English | Comments |
---|---|---|---|
Annealing Temperature | 729.4 - 779.4 °C | 1345 - 1435 °F | Soft; Cooling: Furnace 20°F/hour to 1200°F/ Then air cool; < 235 HB |
Schmolz + Bickenbach Thermodur® 2367 Superclean Hot Work Die Steel Description: Thermodur® 2367 Superclean is an electro slag remelted (ESR) hot work die steel developed for applications where high temperature properties (tensile strength & thermal conductivity).. |
|||
Annealing Temperature | 740.6 - 779.4 °C | 1365 - 1435 °F | Soft; Cooling: Furnace 20°F/hour to 1200°F/ Then air cool; < 170 HB |
Schmolz + Bickenbach Thermodur® E38K Hot Work Die Steel Description: Thermodur® E38K is an electro slag remelted (ESR) modified H-11 die steel, developed for hot working applications where maximum mechanical strength (toughness) properties are require.. |