Polymer Property : Annealing Temperature = 1345 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Annealing Temperature 729.4 - 779.4 °C
1345 - 1435 °F
Soft; Cooling: Furnace 20°F/hour to 1200°F/ Then air cool; < 235 HB
Schmolz + Bickenbach Thermodur® 2367 Superclean Hot Work Die Steel
Description: Thermodur® 2367 Superclean is an electro slag remelted (ESR) hot work die steel developed for applications where high temperature properties (tensile strength & thermal conductivity)..